WC10Ni -45 +11um HVOF HVAF Thermal spraying powder Agglomeration sintering Tungsten carbide 10 nickel
Product Image
Details Image
Design Image
Composition
WC+Ni
Performance Index
ƒ Operating temperatures up to 500 ° C (930 ° F)
Packing Instructions
Bottles, buckets
Description
WC10Ni -53 +20 um HVOF HVAF Thermal spraying powder Agglomeration sintering Tungsten carbide 10 nickel |
ƒ Resistant to hammering, erosion, abrasion and sliding wear
ƒ has higher corrosion resistance and toughness than WC-Co, but lower hardness
ƒ has higher hardness than WC 17Ni, but lower toughness
ƒ Used for ball valve, gate valve, oil field equipment
ƒ Cobalt free: Can be used in radioactive environments
ƒ Operating temperatures up to 500 ° C (930 ° F)
Hot recommended